Material material | Stainless steel |
Item number | MIM1523 |
Product type | Lock accessories |
Powder pretreatment | Screening |
Powder preparation method | Atomization method |
Molding method | powder injection molding |
Mold material | steel mold |
Mold type | Injection mold |
Sintering method | solid phase sintering |
sintering atmosphere | vacuum |
sintering temperature | 1350-1550 |
suppression method | Two-way molding |
Post-processing | heat treatment |
Proofing cycle | 8-15 days |
Processing cycle | 16 days and above |
annual processing capacity | 1000000 |
Annual remaining processing capacity | 400000 |